Hoeveelheid (ton) | 1 - 100 | 101 - 20000 | > 20000 |
Geschatte tijd (in dagen) | 7 | 35 | Overeen te komen |
Wearalloy ar slijtvaste stalen platen chemische samenstelling:
|
||||||
Cijfer
|
Ar400
|
Ar450
|
Ar500
|
|||
Koolstof
|
0.12/0.16
|
0.18/0.26
|
0.27/0.30
|
|||
Mang. (max)
|
1.55
|
1.20
|
0.95
|
|||
Phos. (max)
|
0.025
|
0.025
|
0.025
|
|||
Zwavel (max)
|
0.005
|
0.005
|
0.005
|
|||
Silicium
|
0.35/0.55
|
0.40/0.55
|
0.45/0.55
|
|||
Boor
|
0.0005/0.005
|
0.0005/0.005
|
0.0005/0.005
|
|||
Chroom (max)
|
0.55
|
0.65
|
0.75
|
|||
Nikkel (max)
|
0.35
|
0.35
|
0.35
|
|||
Moly (max)
|
0.55
|
0.60
|
0.65
|
|||
Hardheid (bhn)
|
388-430
|
444-475
|
477-534
|
|||
Opbrengst (psi.)
|
156,000
|
170,000
|
182,000
|
|||
Treksterkte (psi.)
|
194,000
|
206,000
|
235,000
|
|||
Rek in 2”
|
19% - 23%
|
18% - 23%
|
17% - 23%
|
Slijtvaste stalen platen
|
||||
Standaard
|
Typische staalsoorten
|
Dikte (mm)
|
||
Gb/t 24186
|
Nm300/nm360/nm400/nm450/nm500/nm550/nm600
|
≤80
|
||
Har dox
|
Har dox400/450/500/550/600
|
2 ≤ t≤ 130
|
||
Ar
|
Ar400/ar450/ar500/ar550/ar600
|
4 ≤ t≤ 100
|
||
Xar
|
Xar400/xar450/xar500/xar550/xar600
|
4≤t≤100
|
||
Raex
|
Raex400/raex450/raex500
|
2 ≤ t≤ 80
|